Mga sirs! Question,
Possible ba i-top coat ang collinite 476s over collinite 915? Mag bibind ba sila? at kailangan pa ba ng curing period between the 2?
Monthly: Wash > Nanosil/Step 2 > 915 > 476s
Or is it overkill na?
I really liked the look of 915 compared sa 476s, kaso gusto ko kasi sana gawing monthly nalang ang pag wawax coz less contact = less scratches/swirls.
915's looks + 476s' durability =

. Everyday kasi sya nkabilad sa araw (open parking).
-
Btw my regimen is,
Every 6 months: Wash > Clay > KAIO > KSG > 12hrs Curing > Collinite Wax
then Monthly: Wash > Nanosil or Glaze > Wax
every 2-3weeks (situational): Wash > QD
Maraming salamat po sa makakasagot!