Results 1 to 8 of 8
Hybrid View
-
Verified Tsikot Member
- Join Date
- Jul 2003
- Posts
- 35
October 22nd, 2003 12:55 AM #1anong klase ba ng masilya ang maganda gamitin pra sa sasakyan? gusto ko kasi pag-aralan kung panu magmasilya eh thanks!!!!
-
-
-
Tsikoteer
- Join Date
- Oct 2002
- Posts
- 10,620
October 22nd, 2003 03:04 PM #4Glasurit ang Bestseller ko,
Polytuff, Easytite, Polypatch, Yes are good brands also.
A. Prep- Using 16-24 Grit sanding disc, grind or sand all sections of the surfaces to be filled to a clean surface or bare metal completely free from wax, oil, grease, rust, moisture and other foreign materials
B. mixing ratio: 100 parts by weight of bodyfiller to 2-3 parts by Hardener Paste (Red) 100:2-3
C. Application: using the bodyfiller applicator or PALETA or PUTTY KNIFE, firmly and speedily spread a thin layer of filler over the prepared surface area to assure a strong bond, then immediately build up to any desired thickness- by pressing and forming the filler according to the shape of the surface.
allow the applied filler to set hard for about 20-30 minutes after application, then hand sand or machine sand to a smooth texture, after which it is now ready for priming and painting
filing work with hardener should be done as quickly as possible.
pot-life of mixed putty is about 5-6 minutes at 30C degrees
-
Verified Tsikot Member
- Join Date
- Jul 2003
- Posts
- 35
October 26th, 2003 09:51 PM #5thanks sa mga nag-reply and thanks din sir kimpoy for the info. will buy glasurit yun kasi nakita ok avail here sa amin. thanks!!!
-
Verified Tsikot Member
- Join Date
- Jul 2003
- Posts
- 35
October 28th, 2003 06:51 AM #6kimpoy:
1. scrape to metal ko kasi yung pipinturahan ko eh, i used epoxy primer sealer.... after ba ng epoxy apply pa ako ng quick build primer before applying filler???, yun kasi nabasa ko sa car craft na magazine
2. Ill be using sana RM paint mas maganda ba kung RM products din gagamitin ko like: sealer, supergloss thinner, topcoat???
sorry kung daming tanung..... NEWBIE in painting eh....
-
Tsikoteer
- Join Date
- Oct 2002
- Posts
- 10,620
October 28th, 2003 10:28 AM #71.After Scraping the Metal, Thoroughly Clean and dry the area, the apply Epoxy Primer (Zinchromate is more i recommend), allowed to dry overnight and sanded
Apply Bodyfiller to imperfections and dents. Sand well
Apply Putty to minor imperfections. Sand well
Apply (Quick build) Primer over the entire area
allow 2 hours before sanding with 400 Grit
Dry the surface well before applying colorcoat and topcoat.
Goodluck!
2. you can interchange products as long as they are the same type (Arcylic or 1K, Urethane or 2K). but its better practice to use the same brand
HTHLast edited by kimpOy; October 28th, 2003 at 10:30 AM.
-
Verified Tsikot Member
- Join Date
- Jul 2003
- Posts
- 35
November 1st, 2003 01:16 AM #8thanks kimpoy.... yung putty ba na suggest mo yun ba yung red surface glaze kung tawagin o yun yung polytuff.... thanks!!!
naisip ko na lang na maybe its related to the old Nissan CVT issues... kaya siguro they released...